Certification: | BSCI, CE, ISO, RoHS |
---|---|
Technique: | Chopped Strand Fiberglass Mat (CSM) |
Mat Type: | Facing (Surfacing) Mat |
Still deciding? Get samples of US$ 1/Piece
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
OPERFECT™Black fiberglass tissue is used as a facer component in duct insulation systems and provide a smooth surface and acoustical and thermal performance. Black fiberglass veil is suitable as a surface lamination for fiberglass wool and rock wool thermal insulation etc., as well as an acoustic insulation material for wooden or aluminum ceiling panels.
Perfect black fiberglass tissue (nonwoven) is nonwoven composed of glass fibers oriented in a random partern and bonded together with a proprietary, non-facing, black acrylic resin system in a wet laid process. The combination of fibers and binders form the product with high elongation and low dusting characteristics.
We can also add PE coating layer for black fiberglass nonwoven used in the heat sealing process for glass wool/ rock wool industries etc.; Further more, we can also adjust colors, tensile strength, fireproof performances etc. according to customers requirements.
Grammage range: 30 g/m2 to 300 g/m2 |
Roll width: 0.6m to 2.0m |
Roll length: 60m to 1600m |
For the years since it was set up in 2001, Shandong Perfect Corporation has been manufacturing foil lamination, thermal insulation, roofing membranes, and fiberglass products for customers. Our products can make your home, office, or factory more comfortable and energy efficient.
Our company has gained certificates of ISO9001, and ISO14001 quality management and set up strict quality control systems. For our products, FM, CE, TUV, and CCS certificates are needed to develop the markets.
Based on mutual trust and win-win policy, we are pleased to establish long-term cooperation with customers from America, Germany, India, Malaysia, Vietnam, Argentina, Brazil, Saudi Arabia, Greece, etc.
We are committed to providing the Earth with a better and greener tomorrow by putting a stop to climate change with our products.
Our company adheres to the development path of independent innovation and science and technology and pays attention to sustainable green development. Our company has a provincial-level enterprise technology center, a provincial-level new inorganic fiber thermal insulation material engineering laboratory, l Technology Research Institute, a Laboratory, and other R&D institutions. Declared 36 scientific and technological patents, including 8 invention patents and 28 utility model patents, and obtained 3 domestic leading scientific and technological achievement appraisals.
Q: WHAT LAMINATION WAYS DO YOU USE?
A: We have plastic extrusion, and glue laminations with our accurate machines & professional techniques to control the good quality.
The lamination way is according to the customer's requirement or our rich experience.
Q: CAN I ORDER PERFORATED & PRINTED PRODUCTS?
A: Yes, PERFECT can perforate its full line of insulation facings & arrange printing for foils.
Perforations are available in the following options:
Full coverage where 100% of the exposed surface is pin perforated. This is designed for applications where the facing is typically not laminated to the fiberglass.
Pattern or "Channel" perforated to allow for easy laminating. This technique allows the facing to be laminated to fiberglass with no adhesive bleed-through.
Q: WHAT IS THE MAXIMUM INDOOR HUMIDITY THAT AVOIDS MOISTURE PROBLEMS?
A: The maximum recommended continuous indoor relative humidity (RH) varies from 30% to 45%, depending on geographic location. General guidelines by region of the country can be found here. An engineer should be consulted to determine the correct HVAC design for a specific facility.
Q: WHAT HAPPENS WHEN A FACING BECOMES WET AFTER INSTALLATION?
A: Typically, insulation facing will not be affected by limited exposure to water if allowed to fully dry. Prolonged exposure to water can potentially result in a loss of certain physical properties.
Q: WHY DO YOU OCCASIONALLY EXPERIENCE STAINING OF FOIL-FACED INSULATION?
A: Improperly ventilated bags are the primary cause of staining.
Black or brown staining is caused by extended exposure to moisture on the surface of the foil.
Potential sources of moisture are: Adhesive used to laminate the facing to fiberglass, Improper job site storage, Exposure to curing concrete, Daytime/nighttime temperature changes